    Quote Originally Posted by DAFF View Post
    This is the disk I was referring too. 2000/3000/5000

    http://www.autogeekonline.net/forum/...oam-discs.html

    Also, there is a difference between fibreglass polish and automotive stuff. The automotive will work but it will not perform as well in time and is harder to apply.
    Yeah, I know what you were referring to. I have the 3000 grit foam trizect already. But it was going by hand. I could see a difference. I'm going to pick up some for the pneumatic once I finish sanding. I just wondered if you'd tried it with speed on a gelcoat. The grits available (that I can find here) are all the high-end 3m Trizect finishing discs. While they do cut and do a great job. They don't last very long. It took me 8 just to do the bottom front half of the boat. And at $3 a pad, that's pricey.

    Currently I'm doing the bottom hull. It was so bad I had to start with 600 grit, then 1000 grit, 1200, 2000 (by hand), and then 3000 grit foam on the pneumatic. Then compound, polish, and buff.

  2. #12
    Join Date
    Feb 2009
    Location
    Edmond, OK
    Posts
    2,508

    Default

    What I used before and what I'm using again this time is the following...

    3M Super Duty Compound with the 3M wool pad
    3M Perfect-It polish with 3M grey foam pad
    3M Finesse-It finishing glaze with 3M grey foam pad

    I've used a couple different waxes and not sure I'm happy with those. I've been reading a fair amount and it seems like there is a strong concensus supporting the use of the Starbrite Marine Polish with PTFE. I'm going to try that this time as the final "protective" coat.

  3. #13
    Join Date
    Feb 2012
    Location
    Ohio
    Posts
    826

    Default

    I just wanted to bump this thread up so I could find it for a while. I have lightly polished the new boat twice and then waxed and then once back in the water she goes back to been all oxidized. So I need to upgrade what I am doing.
    2006 24SSV 8.1 Vortec

  4. #14
    Join Date
    Nov 2008
    Location
    Walkersville,MD
    Posts
    618

    Default

    Haugy, great thread! I wetsanded my Mariah a couple of years ago to get rid of the oxidation, then used the Meguiars brand of products. They have an 800 number and I called and told them what I was doing. Recommended a three step of #49 oxidation remover, #45 polish, and then the high tech yellow wax. Worked very well for me, and then keep her out of the sun as much as possible...and that does seem dumb as we all want to go out on our boats on sunny days!
    -Rich
    1990 Supra Mariah/351 PCM 1:23-1 PCM

  5. #15
    Join Date
    May 2006
    Location
    Nashville
    Posts
    2,127

    Default

    Quote Originally Posted by gogger View Post
    I just wanted to bump this thread up so I could find it for a while. I have lightly polished the new boat twice and then waxed and then once back in the water she goes back to been all oxidized. So I need to upgrade what I am doing.
    Man I can't get used to the new avatar for you now.

    What are you using for polish? I'm about to try the 3M Finesse it tonight on the bottom of the hull and see how it does. The bottom hull is shiny, but not glossy. I'm hoping this will have enough cut to just be a little bit more than polish, but not a compound.

  6. #16
    Join Date
    Sep 2009
    Location
    Carrollton, VA
    Posts
    265

    Default Re: Polishes, compounds and waxes thread

    2000 Supra Launch. Has Spent the last 6 years with the PO with no cover and no waxing.




    "Buff Magic" metal and fiberglass marine compound. You can find the pint size can, I think that's the size, on Amazon for around $22. This will do a whole 20' boat.

    Apply component on a 4x4 or such area with a disposable paint brush. Layer it on until there is just a light haze of compound covering are.

    Use the edge of your wool pad on your buffer to go side to side, from top to bottom, the up and down, from side to side. now flatten the whole wool pad on the surface and repeat (using the whole pad and not the edges)

    This compound cuts and polishes all at the same time as you'll see in the pictures. These were taken without polish or wax applied.

    I barely wet sanded much and this oxidation was horrid. However I did find that some spots towards the stern were easier to wet sand with 800 and then use the buff magic.

    I have 3M's poly polish but I've yet to apply it.

    I used a 6.5" wool pad. Actually I bought 4. Used 2 while the other 2 were in the wash.




    Sent from my Galaxy Note 2 using Tapatalk

  7. #17
    Join Date
    Sep 2009
    Location
    Carrollton, VA
    Posts
    265

    Default Re: Polishes, compounds and waxes thread

    Final result without wax or polish just yet. Didn't have time but I'll get to it in a few weeks. I was also very surprised at how oxidized the white was. IMO it was worse than the blue.



    Sent from my Galaxy Note 2 using Tapatalk

  8. #18
    Join Date
    Jul 2012
    Posts
    424

    Default

    The 3M Perfect it line is the best. But there are like 10 steps if you go through the whole process... A ton of CC guys have done it and damn, the results are stunning. You can use their boats for mirrors... But there are a few steps you can skip and still get amazing results. All it is is time and money... $$$
    1992 Supra Comp Ts6m 5000 Series PCM 5.8 HO Pro Boss Protec Ignition (not converted) w/ 4010 "Fish Bowl" Carb
    1.23:1 tranny
    "Silent Rider. Quiets The Competition." muffler isn't so silent anymore. ITS HOLLOW!

    1989 Correct Craft Martinique B/R PCM 5.8 Power Plus Package

    1984 E-Scow

  9. #19
    Join Date
    Apr 2012
    Location
    Tacoma, Wa
    Posts
    861

    Default

    The thing about products is find one that works well for you and is easily acquired and stay consistent. I use a Cyclone Orbital and Maguires. The Cyclone uses two 4 inch orbiting gm foam pads that are color coded for aggressiveness. I learned at a detail shop years ago and my station bought a Cyclone years ago for our apparatus. Other than super aggressive cutting ( wet sanding level) I would go with it over a circular buffer. I like Maguires professional because I know the product and it's consistent. I do not like the bottles it comes in though. They get brittle after some shelve life.
    2003 Supra Launch 22SSV
    1986 Ski Natique 2001

  10. #20
    Join Date
    Feb 2012
    Location
    Ohio
    Posts
    826

    Default

    Used the 3m gelcoat restorer. Not much bite. I will try the Finesse next don't need a whole lot of bite, sounds like that might be what I need.